C93200 Bearing Bronze (SAE660) - C932 Leaded Tin Bronze
Short Description:
C93200 Bearing Bronze / High Leaded Tin Bronze has excellent machining properties, good hardness, strength and wear resistance with excellent anti-friction qualities. The alloy is not subject to dezincification and has reasonable corrosion resistance to seawater and brine making it suitable for pump and valve components. C93200 bronze is suitable for bearings, bushings having medium loads and speeds with adequate lubrication.

| Technical Specifications: Copper, Bronze & Brass Sheet / Plate | |||
| Parameter | Copper Sheet / Plate (C11000 / C12200) | Bronze Sheet / Plate (C51000 / C65500) | Brass Sheet / Plate (C26000 / C28000) |
| Material Type | Electrolytic Tough Pitch (ETP) / Phosphorus Deoxidized | Phosphor Bronze / Silicon Bronze | Cartridge Brass / Muntz Metal |
| Standard | ASTM B152 / B11 | ASTM B103 / B96 | ASTM B36 / B19 |
| Thickness Range | 0.016" to 2" (0.4 mm to 50 mm) | 0.016" to 1" (0.4 mm to 25 mm) | 0.016" to 2" (0.4 mm to 50 mm) |
| Width Range | 12" to 48" (305 mm to 1220 mm) | 12" to 36" (305 mm to 915 mm) | 12" to 48" (305 mm to 1220 mm) |
| Length | 48" to 144" (1.2 m to 3.6 m) | 48" to 120" (1.2 m to 3.0 m) | 48" to 120" (1.2 m to 3.0 m) |
| Temper Condition | Soft (O60), Half-Hard (H58), Hard (H80) | Soft (O60), Half-Hard (H02), Spring (H08) | Soft (O60), Half-Hard (H02), Hard (H04) |
| Tensile Strength (Ultimate) | 30 – 38 ksi (210 – 260 MPa) | 47 – 90 ksi (325 – 620 MPa) | 48 – 60 ksi (330 – 415 MPa) |
| Yield Strength (0.5% Ext.) | 10 – 30 ksi (70 – 205 MPa) | 18 – 80 ksi (125 – 550 MPa) | 20 – 45 ksi (140 – 310 MPa) |
| Corrosion Resistance | Excellent | Excellent (marine / saltwater) | Good (moderate) |
| Typical Applications | Bus bars, roofing, gaskets, heat exchangers, electrical components | Bellows, springs, marine hardware, chemical equipment, welding mesh | Radiator cores, decorative trim, architectural panels, musical instruments, ammunition casings |